Chemical reduction of selenates and salirites
Material type:![Text](/opac-tmpl/lib/famfamfam/BK.png)
- T 546.724 S27C
Item type | Current library | Call number | Status | Date due | Barcode | |
---|---|---|---|---|---|---|
![]() |
Mohinder Singh Randhawa Library | T 546.724 S27C (Browse shelf(Opens below)) | Not for loan | 221350 | ||
![]() |
Mohinder Singh Randhawa Library | T 546.724 S27C (Browse shelf(Opens below)) | Not for loan | 221351 |
Browsing Mohinder Singh Randhawa Library shelves Close shelf browser (Hides shelf browser)
The reduction of sodium selenate in alkaline medium has been studied using Na2S03, Na2S04, NaNO2, ZnSO4, Mg(OH)2 and Na2S04, ZnSO4, Mg(OH)2 and zinc dust. The percentage reduction of sodium selenate to sodium selenite by sodium sulphite increases with the